JARO

Article No. B2410-3
Shade Black indigo
Group 4
Spinning, dyeing, weaving, finishing Xingtai H&J Textiles Co. Ltd.
Content 76% Cotton / 24% Tencel
Market Weight oz/yd2 11.2 oz
Yarn Type Warp / Fill: Ring Spun
Finished Ends 69
Dye Type Rope dye
Twill Type 3×1 Right Twill
Cuttable width Inches 60″
Finished Picks 52
Finish Type Regular finish

Order sample meters

Request sample meters to evaluate fabric quality, weight, and performance before production.

Technical specifications

Physical Properties
Test Method Property Average Minimum Maximum
ASTM D-3776 Unwashed Weight (oz/yd²) 11.2
ASTM D-3776 Washed Weight (oz/yd²) 12.1
AATCC 135 % Warp Shrinkage -2 0 -4
AATCC 135 % Fill Shrinkage -2 0 -4
BD Method % Washed Skew Movement 3.5% 3 7
ASTM D-3107 % Elongation -0.4 / -0.3 -3% +3%
ASTM D-3107 % Stretch
ASTM D-3107 % Growth
ASTM D-3107 % Recovery
ASTM D-1424 Rigid Warp Tear (lbs) 16.5
ASTM D-1424 Rigid Fill Tear (lbs) 18.4
ASTM D-5034 Rigid Warp Tensile (lbs) 239.2
ASTM D-5034 Rigid Fill Tensile (lbs) 175.5
AATCC 8 Wet Crocking 1.5
AATCC 8 Dry Crocking 3
Quality
Quality Parameter Value
Maximum Points / 100 yds (Ind Roll) 20
Average Maximum Points / 100 yds (Shipment) 15
Average Major Defects / 100 Linear Yds (Shipment) 4
Washed DE (CMC) 1.5
Processing Notes
Process Notes
Spreading Continuous spread as per increment sheet. Spread tension free to prevent snapback.
Cutting Make pattern adjustments based on shrinkage test data.
Sewing Use 140 chrome medium ball needle and 105 Tex cotton or 90 Tex poly-core thread.
Washing Test wash formula and physical properties before running production.
Care Label Warm wash. No chlorine bleach. Tumble dry low.